Pellentesque non dolor vitae lacus fringilla consequat vel quis enim. Cras venenatis mollis neque in fringilla. In vitae

Recent Posts

Shape

Corundum Mullite Castable

Corundum Mullite Castable is a kind of high strength unshaped refractory materials for sale in RS Company, which can be used in cement kiln. Corundum Mullite Castable Refractory can perform high properties such as high crushing strength, high temperature stability, thermal shock resistance, wear and chemical erosion resistance in lining of large power station boiler and other high temperature equipments.

Application of Corundum Mullite Castable

Corundum Mullite Castable Refractory can be used in steel furnace, cement kiln, glass furnace, iron making furnace, ceramic tunnel kiln and so on.

Corundum Mullite Castable Technique Data

ItemRSCMC-1RSCMC-2RSCMC-3
Al2O3 ≥707585
SiO2 ≤251713
Fe2O3 ≤111
Bulk Density g/cm3 ≥2.72.82.9
0.2MPa Refractoriness Under Load ℃  ≥145014801500
Thermal Shock Resistance, Times, (900℃, water-cooling) ≥252525
Maximum Service Temperature ℃155015501600
Linear Dimensional Change % ≤-0.3-0.2-0.2
Cold Crushing Strength Mpa ≥110℃*24h100110120
1100℃*3h100110120
1400℃*3h115120125
MOR ≥110℃*24h151515
1100℃*3h161718
1400℃*3h171819
Corundum Mullite Castable is a kind of high strength unshaped refractory materials for sale in RS Company, which can be used in cement kiln. Corundum Mullite Castable Refractory can perform high properties such as high crushing strength, high temperature stability, thermal shock resistance, wear and chemical erosion resistance in lining of large power station boiler and other high temperature equipments.

Application of Corundum Mullite Castable

Corundum Mullite Castable Refractory can be used in steel furnace, cement kiln, glass furnace, iron making furnace, ceramic tunnel kiln and so on.

Corundum Mullite Castable Technique Data

ItemRSCMC-1RSCMC-2RSCMC-3
Al2O3 ≥707585
SiO2 ≤251713
Fe2O3 ≤111
Bulk Density g/cm3 ≥2.72.82.9
0.2MPa Refractoriness Under Load ℃ ≥145014801500
Thermal Shock Resistance, Times, (900℃, water-cooling) ≥252525
Maximum Service Temperature ℃155015501600
Linear Dimensional Change % ≤-0.3-0.2-0.2
Cold Crushing Strength Mpa ≥110℃*24h100110120
1100℃*3h100110120
1400℃*3h115120125
MOR ≥110℃*24h151515
1100℃*3h161718
1400℃*3h171819